EXPERIMENTS IN DEAD‐BURNING DOLOMITE AND MAGNESITE1 ...
Stability of calcined dolomite; effect of fineness of raw material, nature of flux and temperature of burning.—Dolomite is difficult to deadburn because the absorption of moisture from the air produces a gradual slacking due, probably, to the hydration of lime and various lime compounds, and this tends to cause all the fluxes tried, 100 mesh raw material gave .